Amorphous bismuth and GO co-doped WO3 electrochromic film with fast-switching time and long-term stability

Dalton Trans. 2024 Feb 6;53(6):2460-2464. doi: 10.1039/d3dt03805j.

Abstract

The sol-gel process for fabricating electrochromic thin films is straightforward, offering advantages such as low cost and ease of compositional control. Herein we prepared GO-Bi-WO3 films with improved electrochromic performance using a simple sol-gel spin-coating method. The sample shows a fast-switching time (1.8 s for coloring and 1.8 s for bleaching), large optical modulation (85% at 630 nm), excellent stability (86.4% retention after 10 200 cycles), and high coloration efficiency (65.9 cm2 C-1). This work indicates the electrochromic performance of WO3-based films can be enhanced by incorporating GO, which provides an effective strategy for the rapid, safe, and efficient fabrication of electrochromic thin films.