Erosion-resistant materials demonstrate low interfacial toughness with ice and superior durability

Mater Horiz. 2023 Oct 2;10(10):4541-4550. doi: 10.1039/d3mh00885a.

Abstract

The strong adhesion of ice to surfaces results in unwanted effects in various industrial activities. However, current strategies for passive ice-phobic purposes lack either scalability or durability, or both, in industrial applications. In this study, erosion-resistant materials, including ceramic-based (WC, SiC, and alumina) and metal-based (a quasicrystalline coating, QC), were studied for their ice-phobic properties via push-off tests with bulk-water ice from -5 to -20 °C. Although their ice adhesion strengths were high (>400 kPa), their interfacial toughness with ice was quite low (1.1 to 2.6 J m-2) and comparable to polymeric surfaces. The force per width required to remove ice on the QC surface was even lower than that of a silicone (Sylgard 184) surface for an ice length of 7.0 cm. The low interfacial toughness of the erosion-resistant materials with ice was also retained after 1000 cycles of linear abrasion under a pressure of 27.0 kPa. The findings of this work expand the material selection options for durable large-scale ice-phobic applications and could enlighten the use of erosion-resistant materials in harsh industrial environments requiring effective de-icing.