Onsite treatment of wastes in municipal waste incinerator: Co-sintering of fly ash and leachate sludge into value-added ceramic granule

Heliyon. 2023 Sep 22;9(10):e20301. doi: 10.1016/j.heliyon.2023.e20301. eCollection 2023 Oct.

Abstract

The leachate sludge (LS) and fly ash (FA) are the foci of hazardous wastes which generated from the municipal solid waste incineration (MSWI). The current work developed a new way to use energy from MSWI process for the on-site sintering of LS and FA at a relatively low temperature. With the assistance of CaF2, granule of LS and MSWI FA were co-sintered. The influence of temperature, the mass of CaF2, and the mass ratio of LS/MSWI FA were investigated. As a result, heavy metals volatilization and leaching in the form of chlorinated salts were controlled. In addition, CaF2 improved the compressive strength of the granule under low-temperature sintering. Moreover, the scale-up co-sintering test was achieved in an MSWI chamber. The results showed that the optimum condition was sintering at 973K for 1 h. The compressive strength of sintered product reached 4.25 MPa, which met the standard of ceramic granule. Moreover, with the addition of CaF2, the volatilization rate of Pb, Zn, and Cd decreased by 6%, 7%, and 6%, respectively. This method can be a promising technique for the utilization of solid wastes.

Keywords: CaF2; Heavy metals volatilization; Leachate sludge; Municipal solid wastes incineration fly ash; Stabilization.