Clinical assessment of class II resin-based composites versus preformed metal crowns performed on primary molars in patients at high risk of caries

Eur Arch Paediatr Dent. 2018 Feb;19(1):39-45. doi: 10.1007/s40368-017-0322-8. Epub 2018 Jan 12.

Abstract

Aim: To compare class II resin composite with preformed metal crowns (PMC) in the treatment of proximal dentinal caries in high caries-risk patients.

Methods: The charts (270) of paediatric patients with proximal caries of their primary molars were reviewed. Success or failure of a procedure was assessed using the dental notes. Survival analysis was used to calculate the mean survival time (MST) for both procedures. The influence of variables on the mean survival time was investigated.

Results: A total of 593 class II resin composites and 243 PMCs were placed in patients ranging between 4-13 years of age. The failure percentage of class II resin composites was 22.6% with the majority having been due to recurrent caries, while the failure percentage of PMCs was 15.2% with the majority due to loss of the crown. There was no significant difference between the MST of class II resin composites and PMCs, 41.3 and 45.6 months respectively (p value = 0.06). In class II resin composites, mesial restorations were associated with lower MST compared to distal restorations (p-value < 0.001).

Conclusions: The MST of resin composites and PMCs were comparable when performed on high caries-risk patients.

Keywords: Caries-risk; Children; Class II resin-based composites; Preformed metal crowns; Primary molars; Survival time.

Publication types

  • Comparative Study

MeSH terms

  • Adolescent
  • Child
  • Child, Preschool
  • Composite Resins / therapeutic use*
  • Crowns*
  • Dental Care for Children*
  • Dental Caries / therapy*
  • Dental Materials / therapeutic use
  • Dental Restoration Failure
  • Dental Restoration, Permanent / methods*
  • Female
  • Humans
  • Male
  • Molar
  • Tooth, Deciduous

Substances

  • Composite Resins
  • Dental Materials