Preparation and application of poly(dimethylsiloxane)/beta-cyclodextrin solid-phase microextraction fibers

J Sep Sci. 2006 Nov;29(17):2684-91. doi: 10.1002/jssc.200600116.

Abstract

A novel poly(dimethylsiloxane)/beta-cyclodextrin (PDMS/beta-CD) coating was prepared for solid-phase microextraction (SPME). The PDMS/beta-CD coating proved to have a porous structure, providing high surface areas and allowing for high extraction efficiency. The coating had a high thermal stability (340 degrees C) and a long lifetime due to its chemical binding to the fiber surface. Polar phenols and amines were used to evaluate the character of the coating fiber by headspace (HS) extraction and thermal desorption, followed by GC-FID analysis. Parameters that affected the extraction process were investigated; these include extraction time and temperature, desorption time, pH, and ionic strength of the solution. For phenols, the range of linearity of the method was 4-500 microg/L and the LOD was 1.3-2.1 microg/L. For amines, the range of linearity was 1-1000 microg/L and the LOD was 1.2-2.8 microg/L. The presence of beta-CD not only increases the thermal stability of the fiber coating, but also enhances its selectivity. Compared with commercially available SPME fibers, the new phases show better selectivity and sensitivity towards polar compounds.