Purpose: This study was to evaluate the fracture resistance of endodontically treated maxillary premolars restored with different CAD/CAM all-ceramic restorations in vitro.

Methods: Mesio-occluso-function tip(MOF) cavities were prepared in 21 extracted human maxillary premolars due to endodontic treatment. The teeth were divided into 3 groups. G1:conventional composite resin; G2: cavities;G3: conventional composite resin with a horizontal glass fiber post inserted palatal walls. Restorations were fabricated from a pressable lithium disilicate glass-ceramic and adhesively cemented (Rely X U200). Then, the specimens were subjected to a compressive load at a crosshead speed of 0.5 mm/min until fracture. The fractured specimens were analyzed to determine the fracture pattern using a stereomicroscope. SPSS 15.0 software package was used to analyse the data.

Results: G3(1570.7±108.7) had higher failure load than G1(1214.6±95.8) and G2(1285.9±87.6)(P<0.05). G1 was similar to G2.The crown was lost in G1 and G2. There was a fracture of the crown and tooth in G3.

Conclusions: CAD/CAM all-ceramic crown with fiberglass posts might be an effective method for restoration of endodontically treated premolars with MOF cavity defect.

MeSH terms

  • Bicuspid
  • Ceramics
  • Composite Resins
  • Dental Restoration Failure
  • Dental Stress Analysis
  • Humans
  • Post and Core Technique*
  • Tooth Fractures*
  • Tooth, Nonvital*

Substances

  • Composite Resins