Low-cost BPO(4) In Situ Synthetic Li(3)PO(4) Coating and B/P-Doping to Boost 4.8 V Cyclability for Sulfide-Based All-Solid-State Lithium Batteries.
Shi J, Ma Z, Wu D, Yu Y, Wang Z, Fang Y, Chen D, Shang S, Qu X, Li P.
Shi J, et al. Among authors: li p.
Small. 2024 Mar;20(13):e2307030. doi: 10.1002/smll.202307030. Epub 2023 Nov 14.
Small. 2024.
PMID: 37964299
Structural damage of Ni-rich layered oxide cathodes such as LiNi(0.8)Co(0.1)Mn(0.1)O(2) (NCM811) and serious interfacial side reactions and physical contact failures with sulfide electrolytes (SEs) are the main obstacles restricting 4.6 V high-voltage cyclability of all-solid-sta …
Structural damage of Ni-rich layered oxide cathodes such as LiNi(0.8)Co(0.1)Mn(0.1)O(2) (NCM811) and serious interfacial side reactions and …