Electrolyte design combining fluoro- with cyano-substitution solvents for anode-free Li metal batteries

Proc Natl Acad Sci U S A. 2024 Jan 30;121(5):e2316212121. doi: 10.1073/pnas.2316212121. Epub 2024 Jan 22.

Abstract

Fluoro-substitution solvents have achieved great success in electrolyte engineering for high-energy lithium metal batteries, which, however, is beset by low solvating power, thermal and chemical instability, and possible battery swelling. Instead, we herein introduce cyanogen as the electron-withdrawing group to enhance the oxidative stability of ether solvents, in which cyanogen and ether oxygen form the chelating structure with Li+ not notably undermining the solvating power. Cyano-group strongly bonds with transition metals (TMs) of NCM811 cathode to attenuate the catalytic reactivity of TMs toward bulk electrolytes. Besides, a stable and uniform cathode-electrolyte interphase (CEI) inhibits the violent oxidation decomposition of electrolytes and guarantees the structural integrity of the NCM811 cathode. Also, a N-containing and LiF-rich solid-electrolyte interphase (SEI) in our electrolyte facilitates fast Li+ migration and dense Li deposition. Accordingly, our electrolyte enables a stable cycle of Li metal anode with Coulombic efficiency of 98.4% within 100 cycles. 81.8% capacity of 4.3 V NCM811 cathode remains after 200 cycles. Anode-free pouch cells with a capacity of 125 mAh maintain 76% capacity after 100 cycles, corresponding to an energy density of 397.5 Wh kg-1.

Keywords: battery; cyano-substitution; electrolyte; fluoro-substitution.