Pseudocapacitive Deionization of Saltwater by Mn3O4@C/Activated Carbon

ACS Omega. 2023 Mar 28;8(14):13315-13322. doi: 10.1021/acsomega.3c00673. eCollection 2023 Apr 11.

Abstract

Capacitive deionization (CDI), a m ethod with notable advantages of relatively low energy consumption and environmental friendliness, has been widely used in desalination of saltwater. However, due to the weak electrical double-layer electrosorption of ions from water, CDI has suffered from low throughput capacity that may limit its commercial applications. Thus, it is of importance to develop a high-efficiency and engineering-feasible CDI process. Manganese and cobalt and their oxides, being faradic materials, have a relatively high pseudocapacitance, which can cause an increase of positive and negative charges on opposing electrodes. However, their low conductivity properties limit their electrochemical applications. Pseudocapacitive Mn3O4 nanoparticles encapsulated within a conducting carbon shell (Mn3O4@C) were prepared to enhance charge transfer and capacitance for CDI. Desalination performances of the Mn3O4@C (5-15 wt %) core-shell nanoparticles on activated carbon (AC) (Mn3O4@C/AC) serving as CDI electrodes have thus been investigated. The pseudocapacitive Mn3O4@C/AC electrodes with relatively low diffusion resistances have much greater capacitance (240-1300 F/g) than the pristine AC electrode (120 F/g). In situ synchrotron X-ray absorption near-edge structure spectra of the Mn3O4@C/AC electrodes during CDI (under 1.2 and -1.2 V for electrosorption and regeneration, respectively) demonstrate that reversible faradic redox reactions cause more negative charges on the negative electrode and more positive charges on the positive electrode. Consequently, the pseudocapacitive electrodes for CDI of saltwater ([NaCl] = 1000 ppm) show much better desalination performances with a high optimized salt removal (600 mg/g·day), electrosorption efficiency (48%), and electrosorption capacity (EC) (25 mg/g) than the AC electrodes (288 mg/g·day, 23%, and 12 mg/g, respectively). The Mn3O4@C/AC electrode has a maximum EC of 29 mg/g for CDI under +1.2 V. Also, the Mn3O4@C/AC electrodes have much higher pseudocapacitive electrosorption rate constants (0.0049-0.0087 h-1) than the AC electrode (0.0016 h-1). This work demonstrates the feasibility of high-efficiency CDI of saltwater for water recycling and reuse using the low-cost and easily fabricated pseudocapacitive Mn3O4@C/AC electrodes.